WRB/Air Barrier Membranes

  • Self-adhered, spun-bond polypropylene
    50 perms Exposure: 180 days
  • Mechanically attached, spun-bond polypropylene
    59 perms Exposure: 180 days
  • Self-adhered, proprietary polyacrylic coating on spun-bond polyester
    26 perms Exposure: 365 days
  • Self-adhered, multiple layers of spun-bond polypropylene
    25 perms Exposure: 180 days
  • 1

UV Stable, WRB/Air Barrier Membranes for Open Joints

  • Self-adhered, spun-bond polyester, UV stable for permanent exposure between open joints
    63 perms Exposure: 365 days
  • Mechanically attached, spun-bond polyester, UV stable for permanent exposure between open joints
    98 perms Exposure: 365 days
  • 1

Rainscreen WRB/Air Barrier Membranes

  • Mechanically attached, multiple layers of spun-bonded polypropylene, factory-bonded rainscreen matrix
    25 perms Exposure: 60 days
  • Mechanically attached, multiple layers of spun-bonded polypropylene, factory-bonded rainscreen matrix
    25 perms Exposure: 60 days
  • Mechanically attached, multiple layers of spun-bonded polypropylene with factory bonded rainscreen matrix
    59 perms Exposure: 180 days
  • Mechanically attached, multiple layers of spun-bonded polypropylene with factory bonded rainscreen matrix
    59 perms Exposure: 180 days
  • 1